TECHNET Archives

October 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 22 Oct 2010 10:32:18 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (182 lines)
Some of window washing fluid can be used for plant food as well (I did).  In the city, along with the big shopping window display, you can have fair amount of the smelly stuff. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Douglas Pauls [mailto:[log in to unmask]]
Sent: Friday, October 22, 2010 10:26 AM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Conformal Coating Board Edges

Yes, I remember Dave Douthit.  I did not always agree with his approaches 
to things, but he did have some interesting data.

The indoor NH3 is not that hard to fathom.  Most of your industrial 
cleaning solutions, especially for glass, have some ammonia in it, so PPB 
levels of NH3 are not unusual.  If you are anywhere in the Midwest in the 
United States, anywhere from April to June, farmers are planting fields 
and most apply anhydrous ammonia during the process.  I am betting Iowa is 
a whole lot higher in NH3 during that time than the PPB range. 

Doug Pauls



Inge <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
10/21/2010 04:51 PM
Please respond to
Inge <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Conformal Coating Board Edges






"Second, how do you determine how harsh an environment  has to be in order 
to coat the edges? "
Dough Pauls

Answer:

Do you remember David Douthit? His definition of Harsh was environments 
that belong to the upper range of the values in the 'OUTDOOR' column. His 
work. There exist no true formulas, but the values below shall in 
principle be multiplied with Temperature, Time, barometric pressure and 
local weather conditions (sun radiation for example). We have in principle 
followed similar figures.

Concentration of selected gaseous air constituents (ppb) in the United 
States.

OUTDOOR

O3          4-43
H2O2     10-30
SO2        1-65
H2S        0.7-24
NO2        9-78
HNO3      1-10
NH3         7-16
HCL         0.18-3
CL2          0.005-0.08
HCHO      4-15
HCOOH   4-20




INDOOR

O3           3-30
H2O2      5
SO2         0.3-14
H2S         0.1-0.7
NO2         1-29
HNO3       3
NH3          13-259
HCL          0.05-0.18
CL2           0.001-0.005
HCHO       10
HCOOH     20

There is one thing I don't understand: NH3 up to 259 ppb indoor.

Hope this gave you at least an idea.

/Inge
































______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2