TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 25 Jun 2002 17:24:06 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Crepeau, Phil" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Crepeau, Phil" <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
this came in just a few days ago.  it's great.

Hi Sunnyliu,
 
You can find a description of the method we use for dye penetrant analysis on our webpage http://www.ivf.se/Elektronik/dye_penetrant/edefault.htm
 
Best regards
Per-Erik Tegehall
 
-----Ursprungligt meddelande-----
Från: sangliu [mailto:[log in to unmask]]
Skickat: den 14 juni 2002 08:45
Till: [log in to unmask]
Ämne: [TN] about the dye penetrant materials in solder joints FA

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2