ASSUMING A SOLDER RESIST IS USED AND IN-LINE STRIPPING IS CARRIED
OUT. ADDITIONALLY, THE DEPOSIT WILL SHOW THE OFF-COLOUR, IF LEAD
CONTAMINATED, UPON EXIT OF THE TAB PLATER.
THX,
LENNY KURUP
On Tue, 25 Nov 1997, Robert Welch wrote:
> Annie,
>
> Since you said oxidized, I'm afraid the condition you describr is due
> to high lead content in the gold bath. Almost all automatic Ni/Au
> machines drag in a small amount of lead into the gold bath,
> regardless of how well everything is run. Because of this the
> gold bath itself must eventually be either treated for lead or
> replaced. I'm realy not sure if there is a functional impact.
> Robert E. Welch
> Process Specialist
> Email: [log in to unmask]
> Modem: 804-239-9120
> Fax: 804-237-3048
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|