Hi Victor-
I was offline for awhile.
The most common problem with laser ablated vias is debris/residue left in the bottom of the hole. Usually it is clear and thin and VERY tough. We use the graphite-based Shadow process for direct plate, so the residue becomes obvious after the panel goes through the Shadow line. Next is the problem of trying to get nice conical sidewalls to make it easy for the plating to go around the bottom edge between the wall and the floor of the via. It is very common to have an acute angle at this juncture, creating something that looks like a crack when it plates. If using a UV laser, you can become over-aggressive in trying to expose lower layer copper, ablating more of the copper than optimal. In this case the base foil could become over-weakened, or you could damage dielectric beneath the foil.
If the via needs to be filled by plating, you will have the usual problems with that: Trying to minimize yet maintain a lap plate so you can get high resolution during the next etching process. Most shops still sand by hand with a block.
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Friday, October 19, 2012 3:04 PM
To: [log in to unmask]
Subject: [TN] PCB/PWB laminate laser abolition
Fellow TechNetters:
Searching for Industry Standards/Guideline for HDI micro vias on the above stated process. The anatomy of a micro via after laser abolition. What are some common anomalies/defects?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
________________________________
Email addresses of ITT Exelis employees have changed from itt.com to exelisinc.com. Please update your favorites and contact information to reflect these changes.
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of Exelis Inc. The recipient should check this e-mail and any attachments for the presence of viruses. Exelis Inc. accepts no liability for any damage caused by any virus transmitted by this e-mail.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|