The majority of ink manufacturers provide a UV cureable ink, such as Taiyo,
Enthone, Lackwerke
Peters etc. Most are applied by squeegee with about a 140/200 mesh screen.
Then cured of course
with UV exposures in the 2000-3000 millijoule range. If you would like
contact names e-mail me personally and I can provide you with some names
----- Original Message -----
From: Lisa Angle <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, November 30, 2000 9:45 AM
Subject: Re: [TN] Removal of UV cured notation
> All,
> I was looking for information on UV curable nomenclature inks,
specifically
> what inks are out there and what are the details for application and
> curing?
> Any information would be appreciated. Thank you.
> Lisa Angle
>
>
>
>
>
> anil k singh <[log in to unmask]>@IPC.ORG> on 11/30/2000 03:56:31 AM
>
> Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please
respond
> to anil k singh <[log in to unmask]>
>
> Sent by: TechNet <[log in to unmask]>
>
>
> To: [log in to unmask]
> cc:
>
> Subject: [TN] Removal of UV cured notation
>
>
> We have to remove cured notation markings on LPISM surface.
> Ink used: ELECTRA UV Curing Legend Printing Ink (Colour: White)
> Is there a formulation that we can use for removing the markings without
> damaging the LPISM surface??
> Thanks in advance
> Linaks Microelectronics Ltd
>
> --------------------------------------------------------------------------
-------
>
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
-------
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|