TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
Date:
Thu, 20 Mar 97 08:24:54 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11228
TO:
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
Resent-Message-ID:
<"GD7xr2.0.p8A.aZJCp"@ipc>
Subject:
From:
"Ron Hollandsworth"<[log in to unmask]>
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w7hig-000BBjC; Thu, 20 Mar 97 07:17 CST
From [log in to unmask] Fri Mar 21 10:
24:52 1997
X-Mailer:
ccMail Link to SMTP R6.00.01
Message-Id:
Parts/Attachments:
text/plain (37 lines)

     Hello TechNet:
     
     We have a .062", board with a top side QFP (SMT) that is reflowing as 
     the board crosses the wave.  Our top side preheat temps have been 
     checked and double checked and is in the 230 degree "F" range.  Peak 
     temps shown as the board crosses the wave are well below the 361 
     degree "F" mark.  We have vias in the pads on some of the leads.  The 
     QFP is plastic.  The board is approximately 3"x5" in size.  Density is 
     maybe a little over average.
     
     Has anyone out there experienced the same thing with some of your 
     products?  We are not seeing a blatant open solder situation, but 
     suttle fractures that will eventually turn to a open situation.
     
     Supposedly the SMT guys profiles are ok.  They are pretty reliable.  
     The boards are inspected after SMT reflow.
     
     What do you think?  Is the reflow caused by the solder coming up 
     through the vias?  
     
     R. Hollandsworth
     [log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2