TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lee parker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Date:
Thu, 4 Nov 2004 16:01:02 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (182 lines)
George

I see our point.

Best regards

Lee
  ----- Original Message ----- 
  From: Wenger, George M.<mailto:[log in to unmask]> 
  To: TechNet E-Mail Forum<mailto:[log in to unmask]> ; Lee Parker<mailto:[log in to unmask]> 
  Sent: Thursday, November 04, 2004 3:19 PM
  Subject: RE: [TN] Immersion Silver


  Lee,
  I missed that it the first time that is why I asked if they wanted 100u" or 100um.  He isn't aking for 100u" of immersion silver he would like immersion silver over 100u" of Ni

  Regards,
  George

  George M. Wenger (908)-546-4531 
  Reliability / FMA Engineer
  Base Station and Subsystems Group
  Andrew Corporation,  40 Technology Drive, Warren, NJ 07059
  [log in to unmask]<mailto:[log in to unmask]>



  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]]On Behalf Of Lee Parker
  Sent: Thursday, November 04, 2004 3:07 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: Re: [TN] Immersion Silver


  James

  100 microinches is far beyond the capability of any immersion process.
  Once the host surface is coated by the attracted material there is no
  long a driving force between the host and the bath. In fact 10
  microinches is normally very difficult. Perhaps the customer is looking
  for electroplated silver.

  Best regards

  Lee

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]] On Behalf Of James Hofer
  Sent: Thursday, November 04, 2004 2:34 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: Re: [TN] Immersion Silver

  Customer states 100 micro inches and the purpose of the NI is due to
  heat
  from the flip chip package.

  James Hofer
  Director of Operations
  Accurate Circuit Engineering
  3019 S. Kilson Dr.
  Santa Ana Ca. 92707-4202
  714-546-2162 work
  714-473-6127 cell
  [log in to unmask]<mailto:[log in to unmask]>
  ----- Original Message -----
  From: "Wenger, George M." <[log in to unmask]<mailto:[log in to unmask]>>
  To: "James Hofer" <[log in to unmask]<mailto:[log in to unmask]>>; <[log in to unmask]<mailto:[log in to unmask]>>
  Sent: Thursday, November 04, 2004 11:33 AM
  Subject: RE: [TN] Immersion Silver


  James,

  Is your customer asking for 100 microns or 100 microinches?  Does you
  customer want this surface finish for soldering or for wirebonding?

  Regards,
  George

  George M. Wenger (908)-546-4531
  Reliability / FMA Engineer
  Base Station and Subsystems Group
  Andrew Corporation,  40 Technology Drive, Warren, NJ 07059
  [log in to unmask]<mailto:[log in to unmask]>



  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]]On Behalf Of James Hofer
  Sent: Thursday, November 04, 2004 1:41 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: [TN] Immersion Silver


  I have a customer asking for Imm Silver over 100um NI. I am concerned
  putting the Silver over the NI as it may lift or peel. This is the first
  time I have had this kind of request. Have any of you well informed Tech
  Heads heard of this before???
  ps. This customer also asked for OSP over the Silver over the NI. I KNOW
  that is not done.

  Thanks for any feedback,

  James Hofer

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text
  in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at:
  http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site
  http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
  for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]>
  or
  847-615-7100 ext.2815
  -----------------------------------------------------
  ------------------------------------------------------------------------
  ----
  --------------------
  This message is for the designated recipient only and may
  contain privileged, proprietary, or otherwise private information.
  If you have received it in error, please notify the sender
  immediately and delete the original.  Any unauthorized use of
  this email is prohibited.
  ------------------------------------------------------------------------
  ----
  --------------------
  [mf2]

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text
  in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at:
  http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site
  http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional
  information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100
  ext.2815
  -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

  ------------------------------------------------------------------------------------------------
  This message is for the designated recipient only and may
  contain privileged, proprietary, or otherwise private information.  
  If you have received it in error, please notify the sender
  immediately and delete the original.  Any unauthorized use of
  this email is prohibited.
  ------------------------------------------------------------------------------------------------
  [mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2