TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Mike McMonagle <[log in to unmask]>
Date:
Fri, 27 Aug 2004 14:51:00 -0500
In-Reply-To:
<A0CF3E6CD78CD411B369009027B0FCFE105D63F7@MIMIR>
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Cal Driscoll <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike McMonagle <[log in to unmask]>
Parts/Attachments:
text/plain (53 lines)
Cal,
        Try Matt Kehoe at Sipad Systems ([log in to unmask]), they are the
US agent for the Siemens SSD process and should be able to help you
through your problems.

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cal Driscoll
Sent: Friday, August 27, 2004 2:38 PM
To: [log in to unmask]
Subject: [TN] 7 year old SSD boards


Hello All-
We have a product we built 7-8 years ago (Before my time) and used SSD
as part of the process.

Today, they want to build 100 of these boards. These boards are SSD and
been sitting in a warehouse for 6 years. This warehouse does not have a
controlled environment. The flux on these boards has leached out into
the paper film.

Question: How can I run-assemble these boards? What should I do to these
boards before running?

Again, thanks in advance for your help.

Cal

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2