No, it will not. We have had same experience. I investigated the boards
myself (years ago)and found no detrimental impact. We asked both Roger and
Taconic why that tarnish, but they had no answers. We changed to Arlon, and
had no further issues. It seems to be a batch dependent phenomenon, because
some batches were not affected at all. We did not dig in that any further.
/Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Kong Hui Poh
Skickat: den 3 december 2007 16:45
Till: [log in to unmask]
Ämne: Re: [TN] [TN} Roger Board turned tarnished affect the performance
Hi Technetters,
I am facing a problem with boards that are of Roger material and was
tin/lead plated.
We subject the boards to reflow, and those area where no solder joint
turned tarnished.
I wander will the signal or frequency be affected by the oxide formed
on the surface.
Thanks.
KH Poh
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|