Funky indeed. Is there a specified reason provided why they feel immersion
tin needs to be applied to inner-layers? I would suspect this is a fab notes
error. As the tin fuses with the copper over time there may be a reliability
issue, I've not heard of, or read any studies on such a process but I would
certainly question this.
As for gold directly on copper, you can expect bonding and reliability
issues with that.
If I were quoting these requirements I would have a long sit-down with the
customer and try to learn why they feel these unorthodox coating methods are
required, I would guess they were written that way in error. If they insist
personally I would no-bid the project.
Franklin
==========================
We are quoting on a PCB which has some unique, at least to us,
manufacturing
requirements and I was hoping that someone might be able to provide
insight
on some of the challenges we foresee.
There are many hurdles to clear with this part, two of which are;
- This 3 layer PCB must have immersion tin plating on all
conductors, inner and outer layers. Does anyone know if the pre-preg will
successfully bond to the immersion tin plated surfaces?
- The outer layers of this part will have areas of selective gold
plating, 50u",plated directly to copper, no nickel interface. Are we
likely
to see problems with bond between the gold and copper?
John Parsons
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentp
age.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori
at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|