Fellow TechNetters:

   I am searching for a clarification on the above stated IPC Standard.   Is there a distinction between wicking and fractures glass rods/laminate.   Is wicking always accompanied by coper plating?   In my experience CAF only requires a laminate integrity anomaly to start the process of migration.   All comments/discussions  welcomed.

Victor,