What is the lead metallurgy and the lead finish?
Best regards,
Leo
Leo M. Higgins III, Ph.D.
Vice President, Technical Operations
ASAT, Inc.
3755 Capital of Texas Highway, Suite 100
Austin, Texas 78704
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Herminia Guevarra
Sent: Friday, April 21, 2006 10:16 AM
To: [log in to unmask]
Subject: [TN] Crack on bend of leads
Hello,
TGIF...but I really need your thought...can you please see attached
pictures and advise what could be the possible root cause of the cracks
on leads?
Thanks,
Herminia
NOT INTENDED AS A SUBSTITUTE FOR A WRITING
NOTHING IN THIS E-MAIL, IN ANY E-MAIL THREAD OF WHICH IT MAY BE A PART, OR
IN ANY ATTACHMENTS THERETO, SHALL CONSTITUTE A BINDING CONTRACT, OR ANY
CONTRACTUAL OBLIGATION BY PNY, OR ANY INTENT TO ENTER INTO ANY BINDING
OBLIGATIONS, NOTWITHSTANDING ANY ENACTMENT OF THE UNIFORM ELECTRONIC
TRANSACTIONS ACT, THE FEDERAL E-SIGN ACT, OR ANY OTHER STATE OR FEDERAL LAW
OF SIMILAR SUBSTANCE OR EFFECT. THIS EMAIL MESSAGE, ITS CONTENTS AND
ATTACHMENTS ARE NOT INTENDED TO REPRESENT AN OFFER OR ACCEPTANCE OF AN OFFER
TO ENTER INTO A CONTRACT. NOTHING IN THIS E-MAIL, IN ANY E-MAIL THREAD OF
WHICH IT MAY BE A PART, OR IN ANY ATTACHMENTS THERETO SHALL ALTER THIS
DISCLAIMER.
This e-mail message from PNY Technologies, Inc. is for the sole use of the
intended recipient(s) and may contain confidential and privileged
information. Any unauthorized review, use, disclosure or distribution is
prohibited. If you are not the intended recipient, please contact the sender
by reply e-mail and destroy all copies of the original message.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|