What is the lead metallurgy and the lead finish? Best regards, Leo Leo M. Higgins III, Ph.D. Vice President, Technical Operations ASAT, Inc. 3755 Capital of Texas Highway, Suite 100 Austin, Texas 78704 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Herminia Guevarra Sent: Friday, April 21, 2006 10:16 AM To: [log in to unmask] Subject: [TN] Crack on bend of leads Hello, TGIF...but I really need your thought...can you please see attached pictures and advise what could be the possible root cause of the cracks on leads? Thanks, Herminia NOT INTENDED AS A SUBSTITUTE FOR A WRITING NOTHING IN THIS E-MAIL, IN ANY E-MAIL THREAD OF WHICH IT MAY BE A PART, OR IN ANY ATTACHMENTS THERETO, SHALL CONSTITUTE A BINDING CONTRACT, OR ANY CONTRACTUAL OBLIGATION BY PNY, OR ANY INTENT TO ENTER INTO ANY BINDING OBLIGATIONS, NOTWITHSTANDING ANY ENACTMENT OF THE UNIFORM ELECTRONIC TRANSACTIONS ACT, THE FEDERAL E-SIGN ACT, OR ANY OTHER STATE OR FEDERAL LAW OF SIMILAR SUBSTANCE OR EFFECT. THIS EMAIL MESSAGE, ITS CONTENTS AND ATTACHMENTS ARE NOT INTENDED TO REPRESENT AN OFFER OR ACCEPTANCE OF AN OFFER TO ENTER INTO A CONTRACT. NOTHING IN THIS E-MAIL, IN ANY E-MAIL THREAD OF WHICH IT MAY BE A PART, OR IN ANY ATTACHMENTS THERETO SHALL ALTER THIS DISCLAIMER. This e-mail message from PNY Technologies, Inc. is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply e-mail and destroy all copies of the original message. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------