Hi Jan - there are lots of pros and cons with the use of water soluable
fluxes. Your use environment, pwa configuration, and type of cleaning
system play important roles in whether you create fuzzy assemblies or
nonfuzzy assemblies. Give Doug Pauls ([log in to unmask]) an email for
additional info.

Dave Hillman
Rockwell Collins
[log in to unmask]





[log in to unmask] on 10/10/97 03:56:03 PM

Please respond to [log in to unmask]; Please respond to [log in to unmask]

To:   [log in to unmask]
cc:    (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject:  [TECHNET] Assy:  Water Soluble Flux




I need a quick education.  The company I have recently hired on at,
would like to immediately change over from RMA flux to Water Soluble
flux for both SMT and thru-hole.  Most of our work is military. It has
been several years since I've researched this topic.
Are SIR tests still required to prove your cleaning methods?
Are SIR tests only required for government contracts?
Can Water Soluble fluxes be used on stranded wire?
Which is a better cleaning process for Water Soluble flux, Batch systems
or in-line systems?
Have most government contractors switched to WS Flux or still using RMA?
Thanks in advance for all responses.
Jan Satterfield
Sr. Process Engineer
L3 Communications
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2