TECHNET Archives

January 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 13 Jan 2016 15:05:58 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (12 lines)
Fellow TechNetters:

   What type of failure mechanism is associated with a HiPot Test Failure on a 750W Switching Power supply?   The visual did not turn up any damage to components exterior structure.   No damage to PWB laminate and solder mash surface.

Victor,


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2