TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Date:
Fri, 5 Jun 1998 10:46:15 EDT
Content-transfer-encoding:
7bit
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (31 lines)
Hello Wolfgang,

     As with Cobey, I've not seen solderballs on bare boards. However, I have
seen what one might consider to be solderballs, but it really wasn't
"solderballing" in the normal sense.

     What had occured on the boards I'm referring to was that the fab had been
HASL'ed and then after the fact, the vias were tented with plugs of mask.
During reflow the plating became liquidous and outgassed thru a break in the
mask and a little ball of solder would form, attaching itself  to the via's
anular pad.

       I couldn't build the second side of the board because I couldn't print
with the balls being attached to the via the way they were. But not only that,
the concern was that there would be contaminates trapped inside the tented
vias.

-Steve Gregory-

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2