Hi Victor - not much data in the public domain on that topic. About the
best you can do is get a copy of the International Tin Research Institute's
Publication 656 titled "Solder Alloy Data". Publication 565 contains
tensile, fatigue and shear data for a number of solder alloys over various
temperature and stress/strain rates. The testing we completed back in the
early 1990's at Rockwell Collins on plated thru hole strength nearly always
resulted in failure of the plated thru hole/laminate rather than the solder
joint itself using slow tensile speeds (unpublished). Plate thru hole
solder joints are truly indestructable.
Dave Hillman
Rockwell Collins
[log in to unmask]
On Fri, Mar 27, 2015 at 3:10 PM, Victor Hernandez <
[log in to unmask]> wrote:
> Fellow TechNetters;
>
> Does anyone have information on the following:
> Finish hole size, lead diameter, solder type, thickness of
> board and lead length. How much force does it require to pull out a lead
> from the solder joint. Will the lead come out cleanly or elongated and
> snap,
>
> Victor,
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|