Hi Gary,
Diodes and transistors have been an issue for years. My
recommendation for diodes and transistors is to use alpha pin numbers in
place of the numerics. It's much easier to map a part to A and C as
opposed to 1 and 2 ( or EBC, rather than 1,2,3). This can cause extra
parts in the library but it typically solves the pinout issue.
-Al Onderick
Gary Bremer <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/27/2007 11:47 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Gary Bremer <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Footprint standards for Polarized components (Diodes)
Steve
Please post this picture on your web site. The Diode D116 pin 1 is
represented by a white dot which is also the anode. I tried to tell the
designers that the bar on the silk screen represents the cathode they
would
not listen so I wound up with major rework to correct all the misplaced
(reversed) components. I was just call to the production line for yet
another problem with F31 again footprint problems. This is why I asked the
question if there exist a standard for creation of component foot prints.
I
do appreaciate all of your replies some have been most enlightening and
will
be passing this information along to the boards designers.
Gary Bremer
Manufacturing Engineer CIT - CID
_________________________________________________________________
Exercise your brain! Try Flexicon.
http://games.msn.com/en/flexicon/default.htm?icid=flexicon_hmemailtaglinemarch07
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|