Try using a hot DI rinse with a ph of no less than 4 for a final rinse,
cut the last h2so4 dip down to 3% and monitor the turnovers in the bath
you should be able to get a very nice bright pink surface where you
don't need any surface treatment before subsequent processing.
Russ
----------
From: Jacob Ransborg
To: [log in to unmask]
Subject: [TN] Cleaning Process after Electroless copper
Date: Thursday, June 18, 1998 1:04AM
Hi technetters
I would like to hear if anybody have experience wtith a cleaning process
of
PCB-boards after plating with electroless copper. Does anybody brush the
boards or use a chemical treatment etc.
Regards
Jacob Ransborg
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|