TECHNET Archives

January 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steven Creswick <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Date:
Tue, 5 Jan 2010 18:13:51 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (76 lines)
Steve,

If you can send me the data sets in an Excel format, I can provide you with
some insight based on magnitude and grouping by Weibull plot.  

If there is a big mix of failure modes, this interpretation will be pretty
generic.  

Its free input, however   :-)

Just send it direct.

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly
Sent: Tuesday, January 05, 2010 4:17 PM
To: [log in to unmask]
Subject: [TN] Pull strength of thermosonic wire bondable gold

Hi All,

I have a wire bond question to the wire bond gurus who have helped me out a
lot in the past. Made 2 versions of a flex circuit - only varied the nickel
thickness. Application is thermosonic gold wire bonding.

Flex circuit lead is .0032 wide - version 1 - nickel is 150 microinches -
soft gold is 50 microinches- pull strength is X

                                                        Version 2 - nickel
is 40 microinches - soft gold is 50 microinches - pull strength is approx.
½X  of version 1-

Is this what I should expect?



Regards Steve Kelly



Steve Kelly (PLEASE NOTE NEW E-MAIL ADDRESS)

(416) 750-8433 (work)

(416) 750-0016 (fax)

(416) 577-8433 (cell)




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2