TECHNET Archives

December 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Yordan Venev <[log in to unmask]>
Date:
Thu, 4 Dec 2003 05:44:56 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (178 lines)
        Yordan:
                There are 11 metals on table 5.1 of the J-Std-001C page
five. You are missing Cadmium,  Arsenic, Silver, Nickel and Bismuth.
                Regards,
                Ramon

> -----Original Message-----
> From: Yordan Venev [SMTP:[log in to unmask]]
> Sent: Thursday, December 04, 2003 2:58 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] SnPb Solder pot composition.
> 
> Ron, Louis, Dale, Edward, Hans, Ramon, Sasha, (hope didn't miss anyone)
> 
> thank you all for the inputs! The analysis was done by means of a scanning
> electronic microscope JEOL JSM 35 CF with X-ray microanalyser TRACOR
> NORTHERN TN-200, and for  samples are used JEOL standards. Parallel to
this
> we have order an analysis of new solder 63/37 (a kind of reliability
check)
> and it showed Sn - 62,37%/ Pb-37,62%. As far as the other materials (Cu,
Au,
> Sb, Fe, Al, Zn) are concerned it seems we have very low level of
> impurities - below 0.01%. Besides the missing Antimony in our analysis,
are
> there other impurities with crucial impact on the solder quality that must
> be checked? Sasha, unfortunately, the still surface of the pot while
taking
> sample is not the case - the sample was drown after the solder was mixed
> well and from the "crest of the wave".
> 
> Yordan
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Edward Szpruch
> Sent: Wednesday, December 03, 2003 4:47 PM
> To: [log in to unmask]
> Subject: Re: [TN] SnPb Solder pot composition.
> 
> 
> Yordan,
> I do have experience with solder wave, only with HASL, but I presume the
> rules are the same:
> -usually the analyses is done to indicate more than 10 materials such as
> Copper, Gold, Antymony, Iron,Silver etc.Those have high influence on both
> metling point and solder joint quality.Limits on such material are really
on
> low level.
> - Concerning Pb - Sn : usually only one of them is analysed, the second
> stated by ballance to 100% .
> The results concerning Pb-Sn are OK, but what with other stuff???
> Edward
> 
> 
> > -----Original Message-----
> > From: Louis Hart [SMTP:[log in to unmask]]
> > Sent: ד דצמבר 03 2003 16:25
> > To:   [log in to unmask]
> > Subject:      Re: [TN] SnPb Solder pot composition.
> >
> > Yordan, I'll leave others to comment on solder joint quality and
> > reliability.  How are the composition analyses done?  I'd bet the
> > measurements are not truly good to 0.01%.  I asked a big solder
> > manufacturer
> > for measurement quality data 2 or 3 years ago, and did not get a good
> > answer.  Lou Hart
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]]On Behalf Of Yordan Venev
> > Sent: Wednesday, December 03, 2003 7:58 AM
> > To: [log in to unmask]
> > Subject: [TN] SnPb Solder pot composition.
> >
> >
> > We have made a composition analysis of our solder wave solder pot and
> > discovered a deviation of the SnPB content. The Sn percentage had gone
up
> > to
> > 65.45% and the Pb content down to 34.54%. I suppose there will be a
> > (small)
> > change in the constitutional behaviour of the alloy - some bigger range
of
> > the liquid-to-solid stage. Except this, what should we be aware of in
> > practice in regards to solder joint quality and reliability? We continue
> > to
> > maintain the pot temperature at 250 deg C (482 deg F).
> >
> > Any inputs will be appreciated!
> >
> > Best regards,
> > Yordan Venev
> >
> > ********************************************************
> > CENTILLION LTD.
> > 7-th km Tzarigradsko shosse Blvd.
> > ATM Center
> > 1784 Sofia, BULGARIA
> > Tel. :(+359 2) 974 47 51, 965 84 95, 965 58 85
> > Fax :(+359 2) 974 47 52
> > mail to: [log in to unmask]
> > www.centillion-bg.com
> >
> >
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
in
> > the BODY (NOT the subject field): SIGNOFF Technet> 
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
http://listserv.ipc.org/archives
> > Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> > for additional information, or contact Keach Sasamori at [log in to unmask]
or
> > 847-509-9700 ext.5315
> > -----------------------------------------------------
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
http://listserv.ipc.org/archives
> > Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> > for additional information, or contact Keach Sasamori at [log in to unmask]
or
> > 847-509-9700 ext.5315
> > -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2