Stainless fibers from an old damaged ESD smock?
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Thursday, June 05, 2008 7:39 AM
To: [log in to unmask]
Subject: Re: [TN] Stainless Steel Contamination Question - Source Nailed!
Dave,
Closest response thus far. If no one guesses correctly, I'll send the
real answer out at 1:00 eastern time. Everyone truly needs to know
this!
Leland
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Simonik, Dave R.
(David)
Sent: Thursday, June 05, 2008 10:24 AM
To: [log in to unmask]
Subject: Re: [TN] Stainless Steel Contamination Question - Source
Nailed!
A brillo pad being used to clean features to aid the vision system?
Dave Simonik
Sanmina SCI
Owego NY Division
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Thursday, June 05, 2008 10:15 AM
To: [log in to unmask]
Subject: Stainless Steel Contamination Question - Source Nailed!
Everyone,
After checking every filter, every transfer belt, every reflow oven, and
most every square inch of the building, I was able to identify the
source of the 10 micron stainless steel that has been giving us such a
headache. Just in case anyone ever has the same problem, I thought I'd
share the solution with our group.
To refresh your memory, we were finding this stuff on top of components,
and later inside our Huntron X-Y table inspection machines. We did
everything but take a hatchet to the Huntrons, and there was nothing
found (of course).
While one of the Huntron machine's operator was gone to lunch, I decided
to check an item she had left behind on her workstation. I took it to
the lab, placed it beneath the microscope, and was astonished to find an
identical match to our contamination woes.
Before I let the cat out of the bag, does anyone want to venture a
guess?
Leland
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for
use by the addressee(s) named herein and may contain legally privileged
and/or confidential information. If you are not the intended recipient
of this e-mail message, you are hereby notified that any dissemination,
distribution or copying of this e-mail message, and any attachments
thereto, is strictly prohibited. If you have received this e-mail
message in error, please immediately notify the sender and permanently
delete the original and any copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS
NOT INTENDED AS A SUBSTITUTE FOR A WRITING. Notwithstanding the Uniform
Electronic Transactions Act or the applicability of any other law of
similar substance and effect, absent an express statement to the
contrary hereinabove, this e-mail message its contents, and any
attachments hereto are not intended to represent an offer or acceptance
to enter into a contract and are not otherwise intended to bind the
sender, Sanmina-SCI Corporation (or any of its subsidiaries), or any
other person or entity.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|