TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 21 Jul 2009 17:12:46 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, stephengregory5849 <[log in to unmask]>
Subject:
From:
stephengregory5849 <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Lou, you're just kidding, right?

There is a method listed for micro-blasting, but doesn't specify doing it 
with walnut shells. Chris says that in his situation he doesn't have access 
to the surface, so micro-blasting (or micro-abrasion) wouldn't be available 
to him anyway.

I sure wouldn't  be using walnut shells because of the ESD. The ESD voltage 
that can be generated with these type of medias are tremendous, and if you 
don't have a system that addresses all the ESD issues, you'll remove the 
coating but probably kill the board.

Steve

----- Original Message ----- 
From: "Louis Hart" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, July 21, 2009 4:47 PM
Subject: Re: [TN] Acrylic CC removal


Chris, my recollection is that IPC-7721 listed methods for removing CCs of 
various types. Haven't looked at it for a few years. I liked the one that 
called for blasting with pulverized walnut shells. Louis Hart

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Tuesday, July 21, 2009 2:52 PM
To: [log in to unmask]
Subject: [TN] [spam] Acrylic CC removal

Hello Netters-

Our customer is in dire need for us to remove acrylic CC quickly and without 
mechanical help (surface is blind to us in an aluminum case).

Destructive testing is to follow. As long as we don't blow through the 
solder mask, we'll be o.k.

Toluene is typically used, but usually requires mechanical help.  No time 
for mail order proprietary blends.

Our quick tests show that D-limonene might be a possibility.

Any thoughts?

Thanks,
Chris

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2