The key is post pumice rinse/clean/dry...the boards need to exit the
machine spotless... and poorly solderable!

Brian

Franklin D Asbell wrote:

> Tony,
>
> Do you have a pumice scrubber? We use an Hyoki aluminum oxide pumice
> scrubber prior to solder mask. Since buying this machine our problems with
> solder mask have dropped off to near nothing.
>
> We did tests some time back when we were evaluating different masks, we
> coated an 18X24 panel after pumice scrub...it came out nice and flat,
> smooth, even, etc etc etc...we could not have achieved those results without
> it I'm sure...
>
> The key is post pumice rinse/clean/dry...the boards need to exit the machine
> spotless...
>
> Franklin
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2