Hi Adrian
It can also be related to the coating thickness you apply, the time you
leave to cure your coating on the board before de-masking and just poor
adhesion of the coating to component or board resist.
If you apply the coat too thick, you leave it to dry too long and it donšt
want to stick then you can be in a real mess. However, if you are just
getting the issue occasionally then these points could be crucial.
Best Regards
Dr Lee Hitchens
SCH Technologies is a Division of SCH Services Limited
Mob: +44 (0) 7862 25 33 21
www.conformalcoating.co.uk <http://www.conformalcoating.co.uk/>
TECHNICAL SUPPORT SERVICE
SCH Services Ltd offers a Technical Support Helpline to help address all
issues relating to reliability. This includes contamination testing,
cleanliness and cleaning issues, plus any coating related questions.
Please contact us via email or telephone:
[log in to unmask] +44 (0)1226 249019 (office hours & answerphone)
+44 (0)7862 253321(out-of-hours emergency)
The opinions expressed in this e-mail are strictly those of the sender and
not of SCH Services Limited. This communication may contain information
which is confidential and may also be privileged. It is for the exclusive
use of the intended recipient(s). Unauthorised use, copying or disclosure
of any of it may be unlawful. If you are not the intended recipient(s)
please note that any distribution, copying or use of this communication or
the information in it is strictly prohibited. If you have received this
communication in error please notify us by e-mail or by telephone (+44
(0)1226 249019) and then delete the e-mail and any copies of it. Virus
Warning - Although steps have been taken to ensure that all email and
attachments are virus-free, we cannot guarantee nor be held liable.
Company Registration: 04043334
Registered office: SCH Services Limited Newburgh Building McLintock Way
Barnsley South Yorkshire S70 6BF
On 03/09/2015 15:43, "Adrian Dimulescu" <[log in to unmask]> wrote:
>Thatšs what wešre doing now, the issue is removing the mask as it will
>occasionally lift a pad or component. Wešre looking to do away with
>masking.
>
>Thanks
>
>
>________________________________
>Adrian Dimulescu | Advanced Engineer | MtronPTI (NYSE MKT: LGL)
>2525 Shader Rd, Orlando, FL 32804
>Office: 407.298.2000
>
>
>
>From: lduso - Diamond-MT.com [mailto:[log in to unmask]]
>Sent: Thursday, September 03, 2015 10:41 AM
>To: TechNet E-Mail Forum; Adrian Dimulescu
>Subject: Re: [TN] Selective Conformal Coat Systems
>
>That low a volume, mask and spray by hand.
>
>
>Lloyd Duso
>Diamond-MT
>Plant Manager
>(814) 535-3505
>www.Diamond-mt.com<http://www.Diamond-mt.com>
>
>On Thu, Sep 3, 2015 at 10:39 AM, Adrian Dimulescu
><[log in to unmask]<mailto:[log in to unmask]>> wrote:
>Hello All,
>
>We're looking into purchasing a small (bench-top type) automated
>selective conformal coat system. This will be used for 100 or so boards
>a week, therefore speed is not an issue. It is important that the system
>is selective as we only want to coat specific areas on the board. I
>wanted to get a feel for what other are using and/or recommend.
>
>Many Thanks
>
>
>
>
>CONFIDENTIALITY NOTICE:
>This email together with any attachments is confidential; intended for
>only the
>recipient(s) named above and may contain information that is privileged or
>exempt from disclosure under applicable law. If you have received this
>email in
>error, or are not the named recipient(s), you are hereby notified that
>any use,
>dissemination, distribution or copying of this email or any attachments is
>strictly prohibited. Please immediately notify the sender and delete this
>email
>and any attachments from your computer. You should not retain, copy or
>use this
>email or any attachments for any purpose, or disclose all or any part of
>the
>contents to any person. The LGL Group, Inc. and its subsidiaries reserve
>the
>right to monitor all email communications through its networks.
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud service.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|