Hi Wayne,
Have not seen the pictures yet, but from your description you got condensation.
Humidity/temperature cycling is a tricky proposition, On heating, you need to heat first before introducing humidity, but even more importantly on cooling you need to first dry the chamber volume before dropping the temperature. Many of the parts within the chamber will lag seriously behind in the temperature changes and you et condensation.
In some past life I did some CAF testing, and setting up and running the humidity/temperature cycling test was a huge challenge needing constant attention. Just making sure that the wet bulb was wet was not simple—you need to gravity feed the water because the pressure in the chamber is elevated.
Werner
-----Original Message-----
From: Thayer, Wayne <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, 26 May 2009 10:01 pm
Subject: [TN] humidity test failure
Hi Technet Gurus!
I have attached a picture of a part responsible for excess current draw during
an extended humidity/temperature cycling test. (I copied Steve so he can
hopefully post!)
The board was carefully solvent cleaned, but no SIR test validating the process
strips all ionic contamination. The board is in an enclosure where plenty of
ionic contaminants are available.
Humidity was supposed to not exceed 90% and was to be non-condensing during
cycling. There were a handful of components which displayed similar deposits on
the same circuit board. These were the only=2
0parts biased during the humidity
test. I believe the evidence suggests at least some condensation occurred. To
me the deposits look like salts. But what do "the experts" think?
Is there any rule of thumb as to humidity levels where we are nuts to try to
survive without conformal coating? Part of the adjacent circuitry contains RF
devices and those guys get panic-stricken when told we probably need to
conformal coat!
Wayne Thayer
This e-mail and any files transmitted with it may be proprietary and are
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those
of the author and do not necessarily represent those of ITT Corporation. The
recipient should check this e-mail and any attachments for the presence of
viruses. ITT accepts no liability for any damage caused by any virus transmitted
by this e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://l
istserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|