Not yet, the 6012 group is likely to include an edge plating requirement in the next version of 6012.
As of now, its user defined. Meaning if you specify edge plating the edge will be plated, thats it (visual evidence of edge plating sufficient for acceptance), unless you define a minimum thickness or other acceptance requirements.
José (Joey) Ríos, Sr QA Engineer
Mission Assurance Manager
Kavli Institute for Astrophysics & Space Research
Massachusetts Institute of Technology
[log in to unmask]<mailto:[log in to unmask]>
(617)324-6272
On Apr 4, 2018, at 10:37 AM, pietro <[log in to unmask]<mailto:[log in to unmask]>> wrote:
Hello expert.
Is there any IPC recommendation/standard about round-edge plating of a PCB ?
Thanks
Pietro
--
Pietro Vergine
President
esd cid+ ESD/CID/CID+/WHMA-A-620Trainer
Leading Edge
Via Delle Attivitá 18
24041 Brembate (Bergamo) - Italy
mobile (+39) 335-5783220
email: [log in to unmask]<mailto:[log in to unmask]>
internet: www.leading-edge.it<http://www.leading-edge.it>
Skype: pietver27
Rispetta l'ambiente: se non ti è necessario, non stampare questa mail.
To respect the environment, if not necessary do not print this email
|
|
|