Angelo,
If all your chemical parameters have been checked and are within the limits
recommended by your supplier, start checking water quality. Nine times out
of ten, discoloration of the oxide coating is a result of poor water
quality. Check pH, cholrides and conductivity.
Jim Kenny
Enthone
Angelo Hermoso <[log in to unmask]>@IPC.ORG> on 05/02/2000 02:26:28 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Angelo Hermoso <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] black oxide discoloration
hi! good morning. i just want to ask what are the other possible causes of
discoloration we are encountering in our line. I already check the
concentration and base from analysis, it is within our standard. I also
check the temperature of the bath tank (chemicals) and it is ok.
Any help would be highly appreciated. Thanks in advance.
angelo
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|