TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Brian Ellis <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Fri, 6 Jan 2006 11:47:03 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (69 lines)
The spec smacks of contact requirements (5 µm Sn/1.3 µm hard Au), not 
for soldering. I'm not convinced that gold-over-tin is a good idea, as 
diffusion will cause intermetallics to form which will cause the gold to 
flake off under mechanical stress. Furthermore, 5 µm tin will not even 
act as a barrier layer to the underlying copper. I believe this is a 
formula for catastrophe in the long term. Like the other person, I'm 
convinced that this is an error, a 5 µm barrier layer of nickel under 
the gold making a LOT more sense.

Brian

Franklin Asbell wrote:
> Received an unusual request for quote with a fab note callout for the
> following.
> 
> 
> 
> 1.      Plate 200/50 microinches SnAu (very hard)
> 
> 
> 
> 
> 
> Now I read that as 200 microinches of tin plating, followed by 50
> microinches of Gold and thought to myself..huhhhh!!!
> 
> 
> 
> I contacted the buyer and he agreed it was quite unusual but they indeed
> need gold over tin. The buyer could not explain why, so I thought I would
> see if others have performed this process, and why such uncommonly mixed
> coatings???
> 
> 
> 
> Franklin
> 
> 
> 
> 
> 
> 
> 
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

-- 
______________________________________________
Please note new e-mail address [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2