Subject: | |
From: | |
Date: | 13 Nov 1996 14:30:47 -0600 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
CLTE is one of their microwave materials. Data sheet shows x=10, y=12,z=40.
Do not see Tg but material is ceramic filled, glass reinforces PTFE.
----------
From: [log in to unmask]
To: [log in to unmask]
Subject: FAB: Arlon
Date: Wednesday, November 13, 1996 1:51PM
Anybody familiar with the board laminate material Arlon-CLTE ? What
are the associated properties such as Tg(degC) ? CTE ppm/degC for X &
Y and the Z axis ?
D.Drake
[log in to unmask]
***************************************************************************