Technet RE: BeCu Flex
Dave, I believe you are requesting information
on berylium copper (BeCu), which is used in flex
circuit applications requiring a well-retained
form or "set". In such applications, the flex
is tooled to be formed once and does not
significantly "relax" like the more ductile
rolled annealed copper.
Half-hard BeCu is well suited to applications
such as flex "cross-overs" and bar soldered
header connectors with flex.
Due to its increased electrical resistance, BeCu
has only about 20% of the current carrying
capacity of rolled annealed copper and must be
derated from standard copper.
Bob Sheldon
>>> David Tyler <[log in to unmask]>
01/19/98 11:19am >>>
Hi Technetters
Does anyone out there have any information on
BuCu for flex circuits. I'm
interested in processing issues both for the
circuit manufacturer and the board
fabricator. Also of interest are the properties
of this material and the
reasons one would choose it. Any information at
all will be greatly
appreciated.
Thanks in advance,
Dave Tyler
##############################################################
TechNet Mail List provided as a free service by
IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full
name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site
(http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar
at [log in to unmask] or 847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|