Kevin
In a former life, I bought similar foil to this, but pure aluminium, in
50 cm wide rolls, from Alusuisse, who are represented in most countries.
However, I think they merged with Alcan last year, so I don't know under
whose banner the Sendzimir rolled products are now sold.
Brian
kevinyeah wrote:
>
> TECHNEThello all:
>
> I want to find aluminum foil supplier.The aluminum specs are: alloy 3003 or 3004, H19 temper [full hard], Degreased, thickness of 0.05mm.If any one can give me some information or idea,please tell me. Thank you at front.
>
> kevinyeah
> [log in to unmask]
> 2001-12-13
> 7w1┘.+-/j膃z獅q胙 隰),HDU NР肚r{ 乢z
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|