TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Scott Westheimer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Scott Westheimer <[log in to unmask]>
Date:
Fri, 19 Jun 2009 16:50:45 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (109 lines)
Loan,

The first photos look like de-wetting. Usually caused by surface contamination and in this cause might be caused by incomplete solder stripping by the supplier. AS long as  they accept paste and reflow they should be OK. The mask issue is caused by the via hole plugging process. What you see is heavier solder mask over the via's and less on the surface. Should not be a problem as long as the pluging material is fully cured and all solvents have been driven out of the via holes.

Regards
Scott B. Westheimer
5709 Clarks Fork Drive
Raleigh, NC 27616
[log in to unmask]
Home: (919)713-0748
Cell NC: (919)961-5364


 




> Date: Fri, 19 Jun 2009 15:48:59 -0400
> From: [log in to unmask]
> Subject: [TN] PCB problems
> To: [log in to unmask]
> 
> Dear Technos,
> 
>  
> 
> I have a few questions regarding a funny lot of PCBs we've received. Steve was kind enough to post the pictures, see
> 
>  
> 
> http://stevezeva.homestead.com/files/non_uniform_hasl.jpg <http://stevezeva.homestead.com/files/non_uniform_hasl.jpg> 
> 
>  
> 
> http://stevezeva.homestead.com/files/non_uniform_hasl_1.jpg <http://stevezeva.homestead.com/files/non_uniform_hasl_1.jpg> 
> 
>  
> 
> http://stevezeva.homestead.com/files/via_halo.jpg <http://stevezeva.homestead.com/files/via_halo.jpg> 
> 
>  
> 
> http://stevezeva.homestead.com/files/via_halo_detail.jpg <http://stevezeva.homestead.com/files/via_halo_detail.jpg> 
> 
>  
> 
> Out of the pack of 15 that I have inspected, most of them have some weird halos around all the vias, but no such issue around the component mounting holes. The pictures show the worst board, the rest have it to a lesser extent. What is it? Should this be a reject? Is this anything we should admonish our fab about?
> 
>  
> 
> Secondly, the SnPb HASL, is irregular on the pads, which is not out of the ordinary, but on some boards looks like in the pictures. I hesitate calling this de-wetting, since the wetting angles are good. Is it de-wetting? Should we reject the boards? I will paste the worst board I find and reflow it, to get an idea what happens during soldering, but I should also be able to help the incoming inspectors draw a line between good and bad in visual inspection of future lots...
> 
>  
> 
> Thank you,
> 
>  
> 
> Ioan Tempea, ing.
> 
> Ingénieur Principal Fabrication / Sr. Manufacturing Engineer 
> 
>  
> 
>  
> 
> 30 ans déjà! - Already 30 years!
> 
> 950 rue Bergar, Laval, Québec, H7L 5A1
> 
> t : 450-967-7100 ext : 244
> 
> Mtl : 514-990-5762
> 
> f : 450-967-7444
> 
> [log in to unmask] <mailto:[log in to unmask]> 
> 
> www.digico.cc <http://www.digico.cc/> 
> 
> P N'imprimer que si nécessaire - Print only if you must
> 
>  
> 
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------

_________________________________________________________________
Microsoft brings you a new way to search the web.  Try  Bing™ now
http://www.bing.com?form=MFEHPG&publ=WLHMTAG&crea=TEXT_MFEHPG_Core_tagline_try bing_1x1
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2