TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
multipart/alternative; boundary="----_=_NextPart_001_01C31BA4.FF0BB650"
Sender:
Subject:
From:
"Black, Paul" <[log in to unmask]>
Date:
Fri, 16 May 2003 08:16:36 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Black, Paul" <[log in to unmask]>
Parts/Attachments:
text/plain (3246 bytes) , text/html (4 kB)
Steve,

I think the delay is necessary. If this job were as important as it sounds,
the OEM should respond quickly. At the same time, if you go ahead and add
the adhesive and it is later rejected by the customer, the delay created to
correct the problem is much more significant and costly.


Thank you,
Paul Black
Manufacturing Engineer
Kronos
E-mail: [log in to unmask]
Voice: (978) 947-1520
Fax: (978) 244-0568
www.kronos.com
Improving the Performance of People and Business(tm)

-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Thursday, May 15, 2003 7:12 PM
To: [log in to unmask]
Subject: Re: [TN] Adhesive where no component is loaded...


There's been some interesting responses! But I'd like to ask a question,
there's been a lot of "what if's" mentioned about having epoxy in between
the pads of the
no-pops, has this really ever caused anybody a problem?

My case was that the work order had already been kitted, we were setting-up,
and then we got an immediate ECO to not populate 20 locations. The stencil
was already made, and due to the locations, taping them off on the stencil
would've caused defects with the print...so I chose to print everything.

Again my question to those who think I should get permission first, would
you accept the delay in delivery by me waiting for you to say if it's okay
or not?

Again, in the fourteen years that I've been doing this, I don't know of any
issue that has arisen of having epoxy between the pads at un-used locations.

By-the-way, I tried my new polyimide stencil today, still not getting enough
height to contact the body of the JANTX diodes with the square
endcaps...back to the drawing board.

-Steve Gregory-

PS Brian, does this email have HTML? I'm not trying to use it...might be my
new version of AOL that I just loaded...

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------


ATOM RSS1 RSS2