TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Glenn Pelkey <[log in to unmask]>
Date:
Wed, 23 Apr 2003 15:49:53 -0700
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (35 lines)
This question comes up a lot, and my recommendation is O.K. for prototype,
not O.K. for production.  You hit one issue with dissimilar metals where
silver and tin don't form an acceptable couple.  You also don't form the
intermetallic, and over time, the oxide on the Sn will form, resistance will
increase, adhesion strength will decrease.  Of course, the operating
environment and reliability expectations need to be considered

Glenn

-----Original Message-----
From: Dan R. Johnson [mailto:[log in to unmask]]
Sent: Wednesday, April 23, 2003 1:04 PM
To: [log in to unmask]
Subject: [TN] SOLDER/EPOXY REACTION


I have a customer who is trying to attach our SMT part to their hybrid
assembly using silver fill epoxy. We use a  lead free alloy (Sn 96.5/Ag
3.5).
Any body have any experiences in this area. The customer (actually the CM)
is worried about dissimilar metals and long term reliability, should they?
Thanks,
Dan

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2