TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Brad Kendall <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 28 Jan 1998 11:52:19 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (30 lines)
Johannes,
     I have read the other responses you have received on this, and agree
with them.  I will just give you my input from my experience.  I studied
this issue when I was setting up the BGA process.  Having attended a BGA
symposium, SMI, etc. and talking with experts at IBM and Motorola I choose
to go with non solder mask defined pads and to print 1:1 with the pad.  We
were also placing PBGA.  With PBGA the ball will melt so you do not need an
excessive amount of paste so 1:1 is fine.  This may be different with
Ceramic.  There are pitfalls to both solder mask defined and non-soldermask
defined, but the non-solder mask defined seem to have fewer issues.  This
is the setup I used and had very good yields and the boards held up very
well under temp/humidity cycling and shock/vibration testing.

Good Luck,
Brad Kendall
Hella Electronics
Michigan SMTA President

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2