You may want to colour-code as well.  Any fluxes used in that process are
labelled yellow, and fluxes for different processes are red or something,
then when they follow Kathy's instruction to remove opposing material they
should be left with all yellow, or all red bottles.  That way you can tell
at a glance whether they have the right materials on their bench.

-----Original Message-----
From: Kathy Kuhlow [mailto:[log in to unmask]]
Sent: December 14, 2001 8:07 AM
To: [log in to unmask]
Subject: Re: [TN] Flux Controls


I would have the flux bottles labeled clearly and then in the process
instructions have the operators remove all opposing fluxes and only have
available the correct flux. The when the work is actually flowing through
walk around and confirm that the operators are following the instructions
and document the random audit.  Communicate, communicate, communicate.....

Kathy

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2