TECHNET Archives

July 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Drew meyer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Drew meyer <[log in to unmask]>
Date:
Thu, 9 Jul 2015 10:25:10 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (14 lines)
Hi All,

I have been forced out from lurking in the shadows and listening to all the great knowledge.  

I have been tasked with providing procurement information for the supplies/materials necessary to test some solder paste attributes at all of our sites.  

Doing fine with stencils and glass microscope slides.  Not finding anything on the copper test coupon for wetting test.

Does anyone know of a source for the coupons ready made?  A plus would be ready made and OSP coated.

If ready made coupons are not available and you are testing solder paste for wetting, what do you use?

Drew Meyer