Subject: | |
From: | |
Reply To: | |
Date: | Fri, 30 Mar 2007 08:20:52 -0400 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
http://www.microwaves101.com/encyclopedia/solderchart.cfm
Go to the chart and see alloy 96.5Sn 3.5Ag
Jim Marsico
EDO Corporation
1250 New Horizons Blvd.
North Amityville, NY 11701
631-630-5079
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Donald Kyle
Sent: Friday, March 30, 2007 8:12 AM
To: [log in to unmask]
Subject: Re: [TN] Soldering using Sn96
Good morning Jim,
Do you have an URL for this CHART that we can look at?
For me Sn96 and gold works like a hose.
Donald Kyle
At 06:58 AM 3/30/2007, you wrote:
>Mornin' Jim!
>
>Really? That's strange...almost every downhole assembly that I've built
>has always been with ENIG plated PCB's...
>
>-Steve Gregory-
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Marsico, James
>Sent: Friday, March 30, 2007 6:46 AM
>To: [log in to unmask]
>Subject: [TN] Soldering using Sn96
>
>Technetters:
>
>
>
>I happened to come across a solder chart from the Indium Corporation
and
>noticed that they do not recommend using Sn96 solder on gold-plated
>surfaces. Can anyone elaborate on this?
>
>
>
>Jim Marsico
>
>EDO Corporation
>
>1250 New Horizons Blvd.
>
>North Amityville, NY 11701
>
>631-630-5079
>
>[log in to unmask]
>
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|