TECHNET Archives

December 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Tue, 31 Dec 2013 16:23:26 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (49 lines)
The caution with laser singulation is that the laser will carbonize the FR-4 along the edge. That is not a concern so long as the copper does not come out into that area.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, December 31, 2013 9:00 AM
To: [log in to unmask]
Subject: Re: [TN] super fine score cuts

Morning Guy,

Wow! 1.24 mil score! I wonder how that was done? Laser? Water-jet?
Here's the pictures:

http://stevezeva.homestead.com/micro_v-score.jpg

http://stevezeva.homestead.com/panel_edge_230x.jpg

From the panel edge photo, it looks like there's no "V" relief to allow for any sort of real singulation in the conventional way that you use a V-score.

Best has a laser that can be used to de-panel something like this:

http://www.solder.net/services/laser-services/

Steve 

-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Tuesday, December 31, 2013 6:31 AM
To: Steve Gregory; 'TechNet E-Mail Forum'
Subject: super fine score cuts

Hi Steve,
We have a 3 inch square panel of 144 little boards. They have the finest little score cuts I have ever seen. 
Each one has a tiny embedded device. I am afraid to break them apart. 
Wondering if you can post the pictures, and if you or anyone on Technet has a good idea for how to singlulate the boards. 

Thanks,
Guy
 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2