TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Brunker Ed <[log in to unmask]>
Date:
Thu, 3 Feb 2000 11:19:33 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, dbrandler <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
dbrandler <[log in to unmask]>
Parts/Attachments:
text/plain (20 lines)
We are looking for a source of 5 micron copper. We want it on a peelable
copper carrier (not aluminum). The problem we have is that the copper
foil manufacturers have become so good that they only supply the thin
foil in roll form without the carrier.  Thanks, Dan Brandler. Ohmega
Technologies.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2