Victor,
I think that qualification of a product means determining that the product /
vendor is capable of meeting your requirements. It's a one-time event that
occurs before purchasing, or on 1st piece. The means used to qualify
usually depend on how critical the part is.
Inspection checks that the product continuously meets your requirements.
It's an event that's repeated each time the product is received.
Good Luck,
Mark Hargreaves
-----Original Message-----
From: Victor Hernandez [SMTP:[log in to unmask]]
Sent: Friday, September 06, 2002 1:57 PM
To: [log in to unmask]
Subject: [TN] Difference in TERMINOLOGY
Fellow TechNetters,
Is there a difference in TERMINOLOGY are is INSPECTION &
RECEIVING the
same as would be a QUALIFICATION of product.
Any HELP with literature and/or industry definition of the two
arenas.
This is a serious subject. I understand that QUALIFICATION
would require all means available to determine probable material
failure and
use of material selection.
Victor G. Hernandez
Component/Material Failure Analysis Eng.
PS4-1, Rm. 132
Ofc: 512-725-3471
Pgr: 512-907-0005
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|