TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Haugaard Svend <[log in to unmask]>
Date:
Mon, 29 Jun 1998 08:42:49 +0200
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Haugaard Svend <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
SMT connectors are just as reliable as leaded connectors. If your former
leaded connector did the job without cracking it's most likely that a
similar SMT connector also will do the job.

Flexing a PCB will most certainly stress the solder joints regardles of
lead or SMT. Lots of books and articles exist concerning this matter but
be sure that it might take some time to get an overview of this. Just
try searching at the web ...

I think there must be a kind of mechanically support to the connector in
order to avoid any load to the solder joints - regardles of connector
type. In this way stress will never arise at the solder joints.
Testing this could e.g. be by means of plugging/unplugging many times to
simulate life cycle - most likely the connector wears out and thus the
press-in force reduces.

Best regards
Svend

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2