BADA,
We track the Defects by area ( SMT, Hand Insertion + Wave Soldering,
Test ). Using a Excel spreadshet we plot graph showing process tendency
( linear graph ) and major causes ( Pareto chart ). Based on pareto
chart we direct our efforts to the big problem. But you have to known
what is commom cause or special cause problems. We deal with special
cause problems only.
Thanks
Jorge Dourado de Santana
Maintenance / Process Engr
Microtec - Brazil
> -----Original Message-----
> From: BADA [SMTP:[log in to unmask]]
> Sent: 26 de Maio de 1999 10:31
> To: [log in to unmask]
> Subject: [TN] Defect Notification
> Sensitivity: Confidential
>
> Hi Techneters,
>
> Like in every company, we have defects that are repaired / reworked in
> production.
> I'd like to collect the data of what is repaired, where, when, by who
> ...
>
> Right now, we are just getting orally a macro data with only the big
> problems
> but I'd like to collect all data (maybe some small problems are there
> all time
> making a lot of rework time).
>
> How is it working in your factory ?
> If you know a system that is easy to use and not taking too much
> labour time,
> please tell me.
>
> Thank you,
> V. Bada
> Process Engineer
> Alcatel Etca
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|