Hi,
Can anyone explain the difference between immersion silver finishings in PCB and selective plating used in leadframe?
What is the difference between the 2 processes?
I am trying to understand why is it that gold wires can be bonded on silver leadframe but does not yield good bond with immersion silver finishings.
Does the thickness of the silver plays a part for good bond with gold wires? Does the grain structure play a part too?
Thanks for sharing.
Best regards,
David.
---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
Version: 6.0.515 / Virus Database: 313 - Release Date: 9/1/2003