Andy, 
When using CB-100,  why do you prefer plasma  at desmear process?

Lourdes

>>> Andy Slade <[log in to unmask]> 04/23 5:08 AM >>>
     Hi Mike,

     The only way we were able to get this under control was to do a flash
     plate immediately after electroless copper dep.  I am assuming that
     you are taking the panels through a permanganate desmear, prior to
     dep.  If you are using plasma alone, this does not provide enough
     surface topography.

     Another option, but it's a costly one, is to pre-fill the vias with
     something like DuPont CB-100.  This accepts metalization better than
     pure resin.  Need to use caution at desmear - must use plasma only.

     Hope this helps...Andy


______________________________ Reply Separator _________________________________
Subject: [TN] Blind Via Adhesion
Author:  Mike Bailey <[log in to unmask]> at smtplink-hadco
Date:    04/22/99 9:01 AM


Got an age old problem.  Maybe there are some new solutions.  We're building
some conventional sub-assy blind via boards that have via in pad
configurations.  No big surprise, the electroless copper adhesion on the
resin-fill areas is blistering.  Re-design using laser drilling is not an
option, nor is direct plate technology or plasma.  We have tried the usual
pre-electroless copper bake as well as post-bake, mechanical scrubbing etc.
etc.  I'm a little hesitant to play with additional desmear tactics as they
have a tendency to or smooth out the original surface texture.

Also as usual, I don't have much time.

Material is conventional 140 Tg epoxy
Hole dia. is .0118.
Yes, some surface sanding is required after final lamination (just like the
rest of you guys)!!

Any ideas?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2