From: TechNet-request
To: ipc
Subject: Galvanic Corrosion
Date: Tuesday, March 25, 1997 4:04PM


Hello technetters,

If a gold finger with splashes of tin/lead on it "does not" make contact
within a gold socket, will there be galvanic corrosion.
Unfortunately IPC-A-600 does not address reliability issues, if there is
reference material out there, I would like to know.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2