     The gold is likely to be impervious.  The substrate nickel, though, 
     will be etched by nitric.  If it is a pattern plate Ni/Au (Ni/Au etch 
     resist) then don't put through nitric strip.
     
     
     Matt Byrne
______________________________ Reply Separator _________________________________
Subject: FAB: Nitric Acid Strip
Author:  [log in to unmask] at SMTPLINK-HADCO
Date:    5/7/97 08:07 PM


     Address,
     
     Is hard/soft gold impervious to a Nitric Acid Strip, if so, how many 
     passes are typically allowed (assuming a gold tab area)?
     
     John Gulley
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2