TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Eli Sarig <[log in to unmask]>
Date:
Thu, 28 Aug 2008 09:16:00 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Reuven Rokah <[log in to unmask]>
Subject:
From:
Reuven Rokah <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Dear Eli,

With zero flow rate, you have only radiation.

The increasing of the flow rate is increasing the air/gas convection and more air/ gas molecules (with heat capacity) flow and cool or heat the substrate.

So you will get radiation and convection in the same time.



Best Regards



Reuven ROKAH

Pls Think green before printing this mail... Thanks



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Eli Sarig

Sent: Wednesday, August 27, 2008 10:24 PM

To: [log in to unmask]

Subject: [TN] Question about heat transfer



My question is related to the heat transfer at the cooling zones. I want to

reduce the substrate temperature from 200º C to 100ºC; can you explain the

relationship between the flowing air temperature and the flow rate? What is

more important: the temperature of the air or the flow rate?

Thanks,

Eli.



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2