TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Fri, 23 Jan 1998 18:04:12 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Thomas E. Waznis" <[log in to unmask]>
Content-type:
text/plain; charset=us-ascii
Subject:
MIME-Version:
1.0
In-Reply-To:
<Pine.SCO.3.95.980123141101.24249A-100000@emxmain>
Content-transfer-encoding:
7bit
From:
"Thomas E. Waznis" <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
>Thank you for the advise Colin.  We are using 2 sheets of 7628 on either
>side and the pressure is 250 PSI -we did try up to 350
>Heat rise is 12 F/min with new paco-pads and 16 when using 1 new with one
>old paco -
pad.

Good start; but I think you will need to get some prepreg with more resin than
any 7628 in there.  :)

Tom Waznis

[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2